หน้าหลัก > บล็อก > เนื้อหา

Performance and application of Gr5ELI high-precision medical Gr23 titanium rod

Oct 11, 2025

The requirements for implant materials can be divided into three aspects: biocompatibility between the material and the human body, corrosion resistance of the material in the human body environment, and mechanical properties of the material.

As a long-term implant material, there are seven specific requirements:

1. Corrosion resistance

2. Biocompatibility

3. Excellent mechanical and fatigue properties

4. Toughness

5. Low elastic modulus

6. Good wear resistance in the assembly

7. Satisfactory price.

1. Industrially pure titanium

2. Ti-6Al-4V and Ti-6Al-4VELi alloys

3. Ti-6Al-7Nb alloy

4. New -type alloys

5. Ti-Ni alloys

 

Gr5ELI High-Precision Medical Gr23 Titanium Rod

 

Gr23 Titanium Rod Specifications: φ4-120mm

Tolerance: 0.03mm

Chemical Composition of GR23: N <= 0.03, C <= 0.08, H <= 0.0125, Fe <= 0.25, O <= 0.13, 5.5 <= Al <= 6.5, 3.5 <= V <= 4.5

Titanium and titanium alloys are widely used in clinical applications to manufacture artificial joints, bone plates, and screws for bone and joint injuries caused by trauma or tumors. They are also used in hip joints (including the femoral head), knee joints, elbow joints, metacarpophalangeal joints, interphalangeal joints, mandibles, artificial vertebrae (spinal orthoses), pacemaker housings, artificial hearts (heart valves), dental implants, titanium-nickel orthodontic appliances, and titanium mesh for skull reshaping.

ASTM F136 TI6AL4V ELI Titanium Bar ASTM F136 TI6AL4V ELI Titanium Bar in stocks

If you are seeking for titanium materials such as titanium plates, bars, tubes, wires and titanium CNC machined parts, BAOJI RELIAB METAL is your one-stop supplier. We supplying the high quality titanium products with fast delivery, and 24-hours sales and after-sales services.

Baoji Reliab Metal Materials Co.,Ltd

Tel: +86-917-8883215

Sales Department 1: +8613092900605 (Mr.Gary)

garychen3215@hotmail.com

Sales Department 2: +8613092913521(Ms. Sophia)

boantj@163.com

Address: No.35 Baoti Rd, Weibin District, Baoji, China

ส่งคำถาม